First simulation of chloride penetration in cracked concrete has been performed. A specimen (top) has been subjected to tension (below it-cracked elements after 15000 steps). Subsequently, it has been subjected to chlorides from the left side. Below are the chloride profiles at 30, 90, 180, 365, and 730 days, respectively. Till next time!